摘要
The accumulation of alkali metals in cryolite electrolyte has negative impacts on the operation of aluminum electrolysis, and part of electrolytes need to be periodically replaced and discharged. A cleaner and efficient process was proposed to recover LiF and Al 2 (SO 4 ) 3 from the waste cryolite electrolyte. Under the optimum sulfated roasting conditions, 87.55% of Li and 30.30% of Al were leached. The obtained cryolite residue with a low molecular ratio could be returned to the aluminum electrolysis system. The addition of sodium benzoate achieved the efficient separation of Al 3+ from Li-containing leachate, and the Al precipitation ratio was 99.78%. Acid leaching of the aluminum precipitate regenerated benzoic acid and recovered 99.62% of Al 2 (SO 4 ) 3 . Finally high-purity cubic LiF was prepared from Li 2 SO 4 solution, and the recovery of LiF was 98.78%.