已核实 DOI 相关产品: 16

Fabrication of SiCw/Ti3SiC2 composites with improved thermal conductivity and mechanical properties using spark plasma sintering

Journal 2020 · IF 2.889 · 9(4): 462-470 · 发表于 2020 年 7 月 9 日
作者: Zhou Xiaobing,Jing Lei,Kwon Yong Duk,Kim Jin-Young,Huang Zhengren,Yoon Dang-Hyok,Lee Jaehyung,Huang Qing
阅读全文 在 PubMed 查看

摘要

High strength SiC whisker-reinforced Ti 3 SiC 2 composites (SiC w /Ti 3 SiC 2 ) with an improved thermal conductivity and mechanical properties were fabricated by spark plasma sintering. The bending strength of 10 wt% SiC w /Ti 3 SiC 2 was 635 MPa, which was approximately 50% higher than that of the monolithic Ti 3 SiC 2 (428 MPa). The Vickers hardness and thermal conductivity ( k ) also increased by 36% and 25%, respectively, from the monolithic Ti 3 SiC 2 by the incorporation of 10 wt% SiC w . This remarkable improvement both in mechanical and thermal properties was attributed to the fine-grained uniform composite microstructure along with the effects of incorporated SiC w . The SiC w /Ti 3 SiC 2 can be a feasible candidate for the in-core structural application in nuclear reactors due to the excellent mechanical and thermal properties.

本研究中使用的阿拉丁产品

16 款产品在本文中被引用