摘要
To obtain chitosan (CTS) with narrower molecular weight distribution, CTS with weight-average molecular weight ( M W ) of 197.30 kDa was first metal complexed and then degraded into five CTSs with M W of 107.90, 56.48, 10.40, 5.67 (CTS-4) and 3.66 kDa. Decrease of M W did not cause a significant change in chemical structure of the residue CTS, but the crystal structure was transformed significantly. The moisture retention increased firstly and then decreased as the M W of CTS decreased. CTS-4 was superior to CTSs with other M W and propylene glycol in terms of the moisture retention. The lower water activity and increase of net isosteric heat were observed in CTS-4, which was due to the migration of immobilized water to a bound-state caused by mounting newly formed chain-end hydrophilic groups per unit weight. CTS-4 could effectively improve moisture retention, showing a potential to substitute commonly used humectant such as propylene glycol.