Degradation behaviour of non-sintered graphene/barium titanate/magnesium phosphate cement bio-piezoelectric composites

Journal 2020 · IF 3.83 · 发表于 2020 年 2 月 4 日
作者: Yufei Tang,Cong Wu,Ping Zhang,Kang Zhao,Zixiang Wu
阅读全文 在 PubMed 查看

摘要

A sintering-free magnesium phosphate cement (MPC) with an arbitrary shape is potentially used as a bone implant material , especially with complex shapes. However, the high degradation rate of MPC may lead to the degradation of mechanical properties . In this study, graphene (G)/barium titanate (BT)/MPC composites were fabricated by introducing the piezoelectric phase BT and conductive phase G into MPC, which exhibited the piezoelectric effect after polarisation. The negative surface of the composite may attract Ca 2+ and Mg 2+ to mineralise rapidly, thereby reducing and improving its degradation rate and mechanical properties, respectively. The contents of additional G and BT were optimised. When BT and G contents were 50 mol% and 0.5 wt%, respectively, the piezoelectric coefficient of the composites increased to 6.31 pC/N, which is an increase of 421% without the addition of G. The results of in vitro degradation and mineralisation in simulated body fluids (SBF) showed that introducing BT and G could effectively slow down the degradation rate, promote mineralisation on the composite surface, and enhance the impact on bone integration.

本研究中使用的阿拉丁产品

89 款产品在本文中被引用