Extraction of SiO2 and Al2O3 from coal gangue activated by supercritical water

Journal 2019 · IF 5.128 · 发表于 2019 年 5 月 27 日
作者: Lina Han,Weiguo Ren,Bing Wang,Xingxing He,Lingjun Ma,Qihuang Huo,Jiancheng Wang,Weiren Bao,Liping Chang
阅读全文 在 PubMed 查看

摘要

In this work, a novel method is introduced to activate coal gangue (CG) for extraction of Si and Al species. The activation experiments were carried out using a stainless steel tube reactor (17 mL) and an autoclave reactor (1000 mL). Firstly, CG was activated by supercritical water added with alkali. It was found that the kaolinite phase of raw CG could be transformed into cancrinite, sodalite and kalsilite by using NaOH, Na 2 CO 3 and KOH as activators, respectively. Secondly, silica (SiO 2 ) and alumina (Al 2 O 3 ) were prepared by acid and alkali combination method. The extraction rates of Al 3+ and Si 4+ from the activated CG using KOH as activator were as high as 78.9% and 69.2%, respectively. The purity of SiO 2 and Al 2 O 3 products were 96.2% and 99.3%, respectively. The as-synthesized SiO 2 both from 17 mL and 1000 mL reactor exhibited very high specific surface areas of 710.0 m 2 ·g −1 and 872.8 m 2 ·g −1 , respectively. In addition, the SiO 2 after hydrophobic modification displayed excellent absorption selectivity for xylene.

本研究中使用的阿拉丁产品

9 款产品在本文中被引用