An advanced core-shell ceramic pebble with Li 4 TiO 4 pure phase core and Li 2 TiO 3 nanostructured shell was prepared by a physical coating method. The phase compositions, morphology and microstructure of Li 4 TiO 4 –Li 2 TiO 3 core-shell ceramic pebbles were investigated. We discovered that using chitosan solution to assist rolling coating helps to improve the coating uniformity of core-shell green pebbles. In addition, the results show that the obtained Li 4 TiO 4 –Li 2 TiO 3 core-shell ceramic pebbles have a diameter of ∼1.1 mm, the shell thickness of ∼13 μm and density of 2.31 ± 0.03 g/cm 3 . It is also noted that the Li 2 TiO 3 shell still maintains the nanostructure (∼80 nm) after sintering. This study provides a feasible method for preparing Li 4 TiO 4 –Li 2 TiO 3 core-shell ceramic pebbles which have a great potential application for the test blanket module (TBM) of International Thermonuclear Experimental Reactor (ITER).