Effective wound dressing based on Poly (vinyl alcohol)/Dextran-aldehyde composite hydrogel

Journal 2019 · IF 4.784 · 发表于 2019 年 4 月 8 日
作者: Ce Zheng,Chunyu Liu,Hailiang Chen,Ning Wang,Xia Liu,Guozhen Sun,Weihong Qiao
阅读全文 在 PubMed 查看

摘要

Wound dressing is of significant importance to promote cutaneous wound healing process. To develop an effective wound dressing, a PVA/DA hydrogel was prepared using a Poly (vinyl alcohol)/Dextran-aldehyde solution blend, followed by crosslinking via freeze-thaw method and freeze-drying. We characterized the hydrogel by infrared spectroscopy, mechanical property tests, swelling behavior test and biocompatibility test. Results showed that the PVA/DA hydrogels had a 3-dimensional, highly porous structure with uniformly distributed pores of 5–10 μm, strong tensile strength of 5.6 MPa, efficient ability to absorb fluid of 6 time its weight and suitable water vapor transmission rate of 2100 g m −2 day −1 to keep a moist environment and good biocompatibility shown by very low hemolysis and no cytotoxicity. In wound healing tests using a full-thickness skin wound model, macroscopic observations showed that the wound covered by the PVA/DA hydrogel almost reached complete healing faster by 10 days, while histological analysis indicated a faster regeneration of skin. Thus, the PVA/DA hydrogel was suitable for application as a wound dressing and may have potential for use in various biomedical applications.

本研究中使用的阿拉丁产品

12 款产品在本文中被引用