已核实 DOI 相关产品: 69

Effect of the pre-reforming by Fe/bio-char catalyst on a two-stage catalytic steam reforming of bio-oil

Journal 2018 · IF 4.908 · 发表于 2018 年 11 月 10 日
作者: Qicong Liu,Zhe Xiong,Syed Shatir A. Syed-Hassan,Zengtong Deng,Xingyu Zhao,Sheng Su,Jun Xiang,Yi Wang,Song Hu
阅读全文 在 PubMed 查看

摘要

Ni-based catalyst is prone to the deactivation by coke deposition during the catalytic steam reforming of bio-oil. In order to optimize catalytic activity of the Ni-based catalyst, a two-stage catalytic reforming scheme was proposed whereby a low-temperature (350–600 °C) pre-reforming process with a less expensive catalyst was introduced prior to the Ni-based catalyst. To study this scheme, the reforming experiments with different combinations of Fe/bio-char (in the first stage) and Ni-Ca/γ-Al 2 O 3 (in the second stage) were conducted. In addition to the quantification of product yields, the tar and gas were characterized with an ultraviolet (UV) fluorescence spectroscopy, a gas chromatography/mass spectrometer (GC/MS) and a gas chromatography (GC). The results indicate that significant proportions of naphthalenes and polycyclic aromatics in the intermediate volatiles turned into furans, phenols and non-aromatics, which are easier to be reformed on Ni-based catalysts, via the Fe/bio-char pre-reforming, resulting in the increase of the final H 2 and CO yields of the overall process. At high pre-reforming temperatures (550–600 °C), the coke formation on Ni-based catalyst was significantly inhibited due to the Fe/bio-char pre-reforming. In addition, the results indicate that the spent Ni-based catalyst had more free NiO and NiAl 2 O 4 spinel than the fresh one, suggesting that the increase in the catalytic activity of Ni-based catalyst during the reforming process was promoted by Fe/bio-char pre-reforming.

本研究中使用的阿拉丁产品

69 款产品在本文中被引用