Selective separation and recovery of iron and tin from high calcium type tin- and iron-bearing tailings using magnetizing roasting followed by magnetic separation

Journal 2016 · IF 1.083 · 发表于 2016 年 7 月 23 日
作者: Zijian Su,Yuanbo Zhang,Jun Chen,Bingbing Liu,Guanghui Li,Tao Jiang
阅读全文 在 PubMed 查看

摘要

In this study, a process of magnetizing roasting followed by magnetic separation, which is used to separate or recover tin and iron from the high calcium type tin- and iron-bearing tailings (containing 35.53 wt.% Fe and 0.56 wt.% Sn), was investigated . A magnetic concentrate containing 66.3 wt.% Fe and 0.07 wt.% Sn with an iron recovery rate of 92.9 wt.% was obtained under optimal conditions: anthracite ratio of 2.5:100, roasting temperature of 850°C, roasting time of 30 min, grinding time of 10 min, and magnetic field intensity of 0.1 T. In addition, the effect of roasting parameters on the separation of iron and tin and phase transformation of SnO2 was investigated by using X-ray powder diffraction, Scanning Electron Microscopy–Energy Dispersive Spectroscopy, etc.

本研究中使用的阿拉丁产品

63 款产品在本文中被引用