Advancing thermo-oxidative stability in silicone rubber with cerium-tin complex oxide

Journal 2024 · IF 3.1 · 35(12): e6591 · 发表于 2024 年 12 月 5 日
作者: Chuanbo Cong,Mingyang Yuan,Han Wang,Rehan Umer,Daigang Peng,Jianglin Ouyang
阅读全文 在 PubMed 查看

摘要

In order to improve the thermal stability of silicone rubber (SR), cerium-tin composite oxides (CeSnO-x) are used as thermo-oxidative stabilizer in phenyl methyl vinyl silicone rubber (PVMQ). CeSnO-x are synthesized via the sol–gel method and characterized by scanning electron microscopy, x-ray diffraction, and X-ray photoelectron spectroscopy (XPS) showing that tin doping led to more oxygen vacancies in CeSnO-x compared to CeO 2 . Through thermogravimetric analyzer, differential scanning alorimetry (DSC) and average activation energy calculation of PVMQ with different thermo-oxidative stabilizer, it was found that CeSnO-8 is outperforming CeO 2 , SnO 2 , and their mixtures in improving the thermo-oxidative stability of PVMQ. In mechanical property tests, due to tin doping, CeSnO-8 exhibit superior performance at all stages during thermo-oxidative aging comparing the different effects of CeO 2 and SnO 2 in different aging stages. XPS of PVMQ composites investigate the mechanism by which CeSnO-8 exhibit different effects. Fourier transform infrared spectroscopy characterizing the Si-C and Si-O bond changes in PVMQ composite before and after aging and the measurement of Mc explore thermo-oxidative stabilizers' role during thermo-oxidative aging of PVMQ. Thermogravimetry-infrared spectroscopy comparisons between unstabilized PVMQ and CeSnO-8-stabilized PVMQ show that CeSnO-8 effectively quenched radicals produced by the oxidation of the PVMQ side group, but exacerbate degradation caused by molecular chain rearrangement.

本研究中使用的阿拉丁产品

6 款产品在本文中被引用