g-C 3 N 4 (CN) based catalysts were effective for photocatalytic ozonation (PCO), but their stability during reaction remained a mystery. This study investigated the change on PCO activity and stability of CN induced by F or I doping. Compared with CN, F-CN had the greater VB potential while I-CN had a greater CB position, which both led to their better O 3 activation. F-CN and I-CN PCO showed the greater oxalic acid (OA) degradation than that of CN PCO process. Though the enhanced activity, both F-CN and I-CN demonstrated the lower stability compared with that of CN. Because of the existing of reactive oxygen species (ROS) like •OH, •O 2 - and h vb + , CN, F-CN and I-CN were partially oxidized, generating NO 3 - and organic molecules such as cyanuric acid. h vb + and •OH mainly accounted for the decomposition of three CN. Triazine ring oxidation resulted in internal tearing and edge fracture as well as the formation of O-containing groups on all CN-based catalysts. O contents in catalysts initially increased and then decreased with reaction time, indicating that surface O-containing groups were unstable. The structural destroy could be eased with the present of organic pollutants. This study deepened the understanding of fate of CN based catalysts during PCO application.
危险品化学品经营许可证(带存储)