Enhanced Catalytic Performance of UiO-67 Supported Pd Catalyst for Toluene Degradation

Journal 2024 · IF 2.3 · 发表于 2024 年 6 月 28 日
作者: Zhao Chunzhi,Mao Dongsen,Meng Tao,Guo Qiangsheng,Yu Jun
阅读全文 在 PubMed 查看

摘要

Owing to the intrinsic nature of the uniformed topologies and ultrasmall Zr 6 nodes of Zr-MOFs, herein, we employed Zr-MOFs (UiO-66 and UiO-67), as opposed to the support of traditional ZrO 2 , to prepare the Pd catalysts for toluene degradation. Compared with the catalysts of Pd/UiO-66 and Pd/ZrO 2 , Pd/UiO-67 catalyst boosted an excellence catalytic performance for toluene degradation, giving the lowest T 90% value of 235 °C with long-term stability. With the assisting of the cavity confinement of Zr-MOFs, Pd nanoparticles are prone to be encapsulated in the 3D frameworks of Zr-MOFs, and the bigger micropores of UiO-67 are more conducive to the formation of larger Pd nanoparticles. The in situ FT-IR results further declared that although the active sites are partly sacrificed due to the larger Pd nanoparticles formed in UiO-67, the stable adsorbed toluene on Pd/UiO-67 boosted the quick degradation of toluene in the reaction interval even without undergoing intermediate processes of benzoate and benzaldehyde. Graphical Abstract UiO-66, UiO-67 and ZrO 2 were employed to prepare the Pd catalysts for toluene degradation, Pd/UiO-67 catalyst boosted an excellence catalytic performance with long-term stability.

本研究中使用的阿拉丁产品

11 款产品在本文中被引用