Fabrication of Si3N4 ceramic balls by SPS method with SiC powder bed

Journal 2024 · IF 1.8 · 21(6): 3842-3850 · 发表于 2024 年 8 月 7 日
作者: Zhen-Quan Liang,Jia-Ji Liang,Jun-Jie Yu,Pei-Bin Cai,Wei-Ming Guo,Hua-Tay Lin
阅读全文 在 PubMed 查看

摘要

Spark plasma sintering (SPS) is an ultrafast sintering method for the preparation of ceramics and ceramic composites with simple geometrical shapes, with the combined application of uniaxial pressure. This study aims to propose an SPS densification method for Si 3 N 4 ceramic balls without necessitating alterations to tools and equipment. The Si 3 N 4 ceramic balls intended for sintering are positioned within a SiC powder bed inside the conventional die used in SPS. The study systematically investigates the effects of presintering temperature (1400°C, 1500°C, and 1600°C) and SPS temperature (1600°C, 1700°C, and 1800°C) on the sphericity, relative density, phase composition, microstructure, and mechanical properties of Si 3 N 4 ceramic balls. Experimental findings reveal that Si 3 N 4 ceramic balls exhibiting an optimal combination of sphericity (0.94 ± 0.02), relative density (98.4%), and mechanical properties (Vickers hardness: 17.5 ± 0.4 GPa, fracture toughness: 6.4 ± 0.1 MPa·m 1/2 ) were successfully achieved at a pre-sintering temperature and SPS temperature of 1600°C, coupled with the use of a SiC powder bed and SPS method. Consequently, the SPS method demonstrates its capability to fabricate Si 3 N 4 ceramic balls with excellent performance.

本研究中使用的阿拉丁产品

14 款产品在本文中被引用