摘要
The flattened bamboo board (FB) has garnered widespread attention recently due to its ability to enhance bamboo utilization and reduce adhesive consumption. However, FB is primarily composed of three macromolecules: cellulose, hemicellulose, and lignin, making it a flammable material. Meanwhile, FB lacks lateral cell tissues, and its relatively low permeability poses challenges for flame-retardant modification. This work introduces an “H 2 O 2 pretreatment-vacuum impregnation-curing” strategy to fabricate the fireproofing of a superior CaCO 3 -mineralized flattened bamboo board (CaCO 3 -FB). The results indicate that H 2 O 2 pretreatment not only enhances the liquid permeability of FB but also maintains a lignin retention rate as high as 69.1 %. The partial retention of lignin, which has a bonding effect, preserves the structural integrity of FB. Cone calorimetry tests show that CaCO 3 -FB significantly reduces peak heat release rate (PHRR), total heat release (THR), peak smoke production rate (PSPR), and total smoke production (TSP) by 34.6 %, 52.9 %, 22.2 %, and 53.6 %, respectively. Overall, the production of flame-retardant FB is successfully achieved through the partial retention of lignin and mineralization of CaCO 3 , which holds great potential to drive significant advancements in the bamboo industry.
危险品化学品经营许可证(带存储)