Moderate dehydrofluorinated PVDF (MD PVDF) composed of polyene and untreated PVDF was produced by elimination reaction in polyvinyl pyrrolidone (PVP) and KOH aqueous solution. Dielectric films of MD PVDF were fabricated by solution casting method to study the energy density performance of the polymer. The energy density of MD PVDF was enhanced and the maximum energy density was 10.5 J/cm 3 at 450 kV/mm with an efficiency of 46%. The enhanced energy density was attributed to combined effects of high conductivity of polyene and charges blockage of untreated PVDF. This work may provide a new way to enhance the energy density performance of polymer dielectrics by moderate dehydrofluorination.