The pure silicon MWW were synthesized for the first time by means of a dry-gel conversion method utilizing N, N, N-trimethyl-1-adamantyl ammonium hydroxide and hexamethyleneimine as the structural directing agents. A vapor transport assisted crystallization method for obtaining complete crystallinity was developed to replace the traditional dry-gel conversion methods. TiCl 4 acid solution treatment was cleverly used for the implantation of titanium in MWW. Compared with Ti-ERB-1, the Ti content of boron- free Ti-MWW is only 20% of the former, the conversion rate of 1-hexene epoxidation is 2.3 times of the former and nearly 100% of H 2 O 2 efficiency.