已核实 DOI 相关产品: 0

Hydrophobic Modification of Small-Pore Pd-SSZ-13 Zeolites for Catalytic Methane Combustion

Journal 2024 · IF 2.8 · 发表于 2024 年 3 月 29 日
作者: Wang Xinyu,Xu Xin,Xiong Wuwan,Ye Daiqi,Chen Peirong
阅读全文 在 PubMed 查看

摘要

Catalytic oxidation is an effective solution for the control of methane (CH 4 ) emission in exhausts from natural gas vehicles. Pd-based small-pore zeolites (such as Pd-SSZ-13) are considered to be the most active catalysts for CH 4 oxidation, but H 2 O in the exhausts tends to induce deactivation of Pd catalysts. In this work, we tuned the hydrophobicity of Pd-SSZ-13 as a representative to improve its H 2 O resistance in CH 4 oxidation. Pd-SSZ-13 catalysts with different Si/Al ratios were obtained by dealuminizing the pristine SSZ-13 zeolite with acid followed by Pd ion exchange, and a reduction of T 50 (i.e. the temperature to reach 50% conversion of CH 4 ) by 20 ℃ was achieved in CH 4 oxidation in the presence of 10 vol.% H 2 O. Detailed physicochemical characterizations showed that the fraction of highly dispersed PdO species (highly active in CH 4 oxidation) increased, whereas that of less inactive PdO x clusters decreased, in the Pd-SSZ-13 after acid modification. In addition, the increase of zeolite hydrophobicity after acid modification alleviated the H 2 O inhibition effect on the active PdO phase, leading to a less activity loss of Pd-SSZ-13 in CH 4 oxidation. The improved hydrophobicity also favored C 3 H 8 combustion over Pd-SSZ-13. These results suggested that simple acid modification could tune effectively the Si/Al ratio and hydrophobicity of zeolite supports, and eventually the physicochemical properties and oxidation performance of the supported Pd catalysts.