Thermoelectric materials convert thermal energy into electricity directly. Constructing nanostructured composite architectures can be an effective strategy to develop thermoelectric performance. SnSe/Ti 3 C 2 composite materials were synthesized through the electrostatic self-assembly method followed by spark plasma sintering. The interfaces introduced by Ti 3 C 2 can scatter carriers effectively, thus increasing the Seebeck coefficients ( S ), finally, a high absolute S value of ~ 296.2 µV K −1 was obtained at 773 K. At the same time, the high-density interfaces of SnSe/Ti 3 C 2 composites enhance the phonon scattering, a low lattice thermal conductivity k lat of 0.54 W m −1 K −1 was obtained. Benefit from the elevated Seebeck coefficient and decreased thermal conductivity, a ZT of 0.1 was obtained at 773 K along the pressing direction, compared with the pure SnSe, the thermoelectric performance improved by 68%. This research will provide a new way for the development of the thermoelectric properties of polycrystalline SnSe.