摘要
Corrosion induced by the geometric crevice potentially threatens safe service of Nickel(Ni)-based GH3535 alloy in Generation IV Molten Salt Reactor System. However, very few studies shed light on crevice corrosion of Ni-based alloy in molten fluoride salt and corresponding mechanism remains unclear. This work investigates the crevice corrosion of Ni-based GH3535 alloys exposed to the 700 °C FLiNaK salt for varied durations from 100 h to 800 h through static corrosion immersion tests. The results of cross sectional morphologies reveal that corrosion depth of depleted alloying elements outside the crevice increases from 38 μm to 59 μm when the corrosion exposure duration increases from 100 h to 800 h. However, the alloy part inside crevice merely exhibits weak corrosion dissolution and almost no depletion of alloying elements can be observed. While the alloy part at crevice mouth suffers from severe corrosion attack and exhibits a stripe-shaped corrosion morphology, which is possibly due to the gradient-driven diffusion and accumulation of oxidative metal ions at the mouth under the concentration difference. Both the depth and width of crevice corrosion at crevice mouth for GH3535 alloy increase with prolonging the exposure duration in molten fluoride salt.
危险品化学品经营许可证(带存储)