Acid sludge, a hazardous waste from lead (Pb) and zinc (Zn) smelting process, commonly contains low-boiling-point elements such as Pb and fluorine (F). However, the complex phase composition of acid sludge typically results in low recovery efficiencies of Pb and F. Herein, we proposed an efficient recovery method for Pb and F through synergistic leaching using a solution containing aluminum ions (Al 3+ ) and chloride ions (Cl − ) followed by stepwise precipitation involving PbCl 2 cooling crystallization and cryolite formation. The single-factor experiment results showed the leaching efficiencies of 98.37% and 92.35% for Pb and F, respectively, which is superior to that of the separate leaching of Pb or F process, due to the intermingle structure of Pb and F phases in acid sludge. The precipitation efficiencies reached 94.44% for Pb and 97.88% for F, and the obtained PbCl 2 and cryolite products meet national standards. Density functional theory (DFT) calculations revealed the chemical states of Al 3+ , calcium ion (Ca 2+ ), and F − in leaching solution and their coexistence mechanism, and thermodynamic analysis clarified the preferential precipitation of cryolite with high quality. Further, the Life Cycle Assessment (LCA) and economic evaluation were conducted for the entire recovery process, indicating the significantly economic and environmental benefits with a cost of only ¥1.61 for treating 100 g of acid sludge. This study provides an efficient and sustainable method for recovering Pb and F from acid sludge, which not only mitigates environmental hazards but also enhances resource valorization, thereby supporting the development of a circular economy in the non-ferrous metal industry.
危险品化学品经营许可证(带存储)