CERAMICS INTERNATIONAL
·
2021
·
IF 4.527
Xin Liu,Mengmeng Fan,Xuguang Zhu,Zengguo Tian,Xin-Jian Li,Hongzhang Song
Bi 2 Sr 2 Co 2 O y with excellent thermoelectric properties has received extensive attention from scientific researchers. In this study, Bi 2 Sr 2 Co 2 O y ceramic samples were prepared using the solid-phase sintering method. By Ag + substitution for Bi 3+ , the hole concentration and electrical conductivity were optimised. On this basis, nano-SiC particles were introduced to increase grain boundaries, improve phonon scattering, reduce the mean free path of phonons, and reduce the lattice thermal conductivity . A sample with a nominal composition of Bi 1.8 Ag 0.2 Sr 2 Co 2 O y + 0.025 wt% SiC had a maximum ZT value of 0.35 at 923 K, which was approximately 67 % higher than the ZT value of pure Bi 2 Sr 2 Co 2 O y . These results confirmed that under the combined action of Ag substitution and SiC doping, the thermoelectric performance of Bi 2 Sr 2 Co 2 O y was significantly improved.
研究领域:
材料科学
·
热电材料研究
✓ 已验证
产品关联
DOI
高影响因子
APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING
·
2024
·Vol. 130
·期 3
·203
·
IF 2.5
Xu Yingying,Xia Siyi,Zhang Yingjiu,Song Hongzhang,Liu Shaohui,Hao Haoshan
In this study, ceramic samples of Bi 2 Sr 2 Co 2 O y + v wt% B 2 O 3 ( v = 0.0, 0.1, 0.2, 0.3, 0.4) were synthesized using the solid state reaction method, and the influence of B 2 O 3 additive on their microstructure and thermoelectric properties were investigated. On one hand, the B 2 O 3 additive acted as a sintering aid, enhancing carrier mobility. On the other hand, B 2 O 3 dispersion served as a nano-second-phase, increasing hetero-interfaces and strengthen phonon scattering, thereby effectively suppressing lattice thermal conductivity. By dual optimization of both electric and thermal transport performance, the Bi 2 Sr 2 Co 2 O y + 0.3 wt% B 2 O 3 sample achieved a high ZT value (thermoelectric figure of merit) of 0.31 at 923 K, which was improved by approximately 33% compared with the pristine Bi 2 Sr 2 Co 2 O y sample.
研究领域:
材料科学
·
凝聚态物理
·
无机非金属材料
·
热电材料
✓ 已验证
DOI
高影响因子
Materials Research Express
·
2018
·Vol. 5
·期 4
·045510
·
IF 1.151
Qiujun Hu,Kunlun Wang,Yingjiu Zhang,Xinjian Li,Hongzhang Song
The thermoelectric properties of Bi2Sr2Co2Oy + x wt% nano SiC (x = 0.00, 0.025, 0.05, 0.1, 0.2, and 0.3) prepared by the solid-state reaction method were investigated from 300 K to 923 K. The resistivity can be reduced effectively by adding a small amount of SiC nano particles, which is attributed to the increase of the carrier concentration. At the same time, the Seebeck coefficients can be improved effectively due to the energy filtering effect that low energy carriers are strongly dispersed at the interface between the SiC nano particles and the matrix. The decrease of thermal conductivity is due to the increase of the scattering ability of the phonons by the SiC nanoparticles distributed at the boundary of the matrix. As a result, the Bi2Sr2Co2Oy + x wt% SiC composites exhibit better thermoelectric properties. The maximum ZT value 0.24 is obtained when x = 0.05 at 923 K. Compared with the sample without SiC nano particles, the ZT value is increased by about 59.7%.
✓ 已验证
DOI
高影响因子
MODERN PHYSICS LETTERS B
·
2019
·
IF 0.929
Y. Zhang,M. M. Fan,C. C. Ruan,Y. W. Zhang,X.-J. Li,H. Z. Song
Bi 2 Sr 2 Co 2 O y ceramic samples have a structure similar to phonon glass electronic crystals, and their thermoelectric properties can be effectively adjusted through repeated grinding and sintering. The results show that multi-sintering can make their grain refined and increase their grain boundary, which will effectively increase density and phonon scattering. Finally, multi-sintering can reduce the resistivity and thermal conductivity, thus obviously improve thermoelectric figure of merit ( Z T ) of Bi 2 Sr 2 Co 2 O y . The optimum Z T value of 0.26 is achieved at 923 K by the third sintered sample.
研究领域:
材料科学
·
热电材料
·
无机非金属材料
·
凝聚态物理
✓ 已验证
DOI
高影响因子
THIN SOLID FILMS
·
2013
·
IF 1.604
Shufang Wang,Shanshan Chen,Guoying Yan,Fuqiang Liu,Shouyu Dai,Jianglong Wang,Wei Yu,Guangsheng Fu
c-axis oriented nanocrystalline Bi 2 Sr 2 Co 2 O y thin films with the average grain size of 25 nm have been achieved by chemical solution deposition combined with a rapid annealing process in oxygen. The resistivity and Seebeck coefficient of the nanostructured films are about 7.0 mΩ·cm and 171 μV/K at 873 K, resulting in a power factor 2–3 times larger than that of the best reported value in the coarse-grained Bi 2 Sr 2 Co 2 O y polycrystalline bulks. Since the thermal conductivity can be greatly reduced due to the increased phonon scattering at the grain boundaries of nanocrystalline films as well as at film surface and at film/substrate interface, great improvements in the ZT are expected in the nanocrystalline Bi 2 Sr 2 Co 2 O y thin films .
研究领域:
材料科学
·
凝聚态物理
·
无机非金属材料
·
能源材料
✓ 已验证
DOI
高影响因子
CERAMICS INTERNATIONAL
·
2025
·
IF 5.6
Yingying Xu,Mengyao Li,Yingjiu Zhang,Hongzhang Song,Haoshan Hao
A series of Bi 2 Sr 2 Co 2 O y (BSCO), Bi 2 (Sr 2/3 Ba 2/3 Ca 2/3 )Co 2 O y (BSBCCO), Bi 1.9 Cu 0.1 (Sr 2/3 Ba 2/3 Ca 2/3 )Co 2 O y (BCSBCCO) and Bi 1.8 Ag 0.2 (Sr 2/3 Ba 2/3 Ca 2/3 )Co 2 O y (BASBCCO) ceramic samples were prepared to optimize the thermoelectric properties of BSCO by high entropy doping combined with Cu/Ag doping. High entropy doping improves the carrier mobility significantly, due to a sintering effect in liquid phase and an additional conduction path. Cu/Ag acceptor doping increases the carrier concentration and Seebeck coefficients. Both them enhance the electrical transport performance of doped samples effectively. Specially, the random distribution of several different cations caused by high entropy doping and Cu/Ag doping can enhance the phonon scattering, which greatly reduces the thermal conductivity of doped samples. Finally, the thermoelectric figure of merit ( ZT ) value of the BASBCCO sample is improved to 0.36 at 923 K on the basis of high entropy doped BSBCCO ( ZT = 0.28 at 923 K), which is twice that of the pristine sample.
研究领域:
材料科学
·
热电材料
✓ 已验证
产品关联
DOI
高影响因子