摘要
NASICON type Li 3 Zr 2 Si 2 PO 12 can be synthesized via cation exchange method with Na 3 Zr 2 Si 2 PO 12 as precursor, which retains the skeleton structure and achieves an ionic conductivity higher than 3 mS cm −1 at room temperature. However, large-scale fabrication via cation exchange reaction seems unlikely considering the expensive precursors and complicated preparation process. Herein, the viability of solid-state reaction to prepare Li 3 Zr 2 Si 2 PO 12 is explored, which has important implication for its industrialization. The sintering was conducted using the raw materials of LiOH, SiO 2 , ZrO 2 and NH 4 H 2 PO 4 with the nominal stoichiometric ratio of Li 3 Zr 2 Si 2 PO 12 . The results show that the final product is a Li 3 PO 4 ·2ZrSiO 4 composite with negligible Li + conductivity, other than the expected Li 3 Zr 2 Si 2 PO 12 with high Li + conductivity. Combined with thermodynamic calculations based on density functional theory (DFT), the competition between Li 3 PO 4 ·2ZrSiO 4 and Li 3 Zr 2 Si 2 PO 12 with NASICON phase is analyzed. It was found that the formation energy (Δ G ) of Li 3 PO 4 ·2ZrSiO 4 is lower than that of Li 3 Zr 2 Si 2 PO 12 . In addition, the decomposition of Li 3 Zr 2 Si 2 PO 12 with Li 3 PO 4 ·2ZrSiO 4 as products is a thermodynamically spontaneous reaction. The influences related to the coordination structures on the structural stability of NZSP are discussed as well. These results demonstrate that the fabrication of Li 3 Zr 2 Si 2 PO 12 through high-temperature sintering is difficult, and the development of a synthetic method with mild conditions is essential for the Li 3 Zr 2 Si 2 PO 12 preparation.
危险品化学品经营许可证(带存储)