已核实 DOI 相关产品: 0

Chemically produced tungsten–praseodymium oxide composite sintered by spark plasma sintering

Journal 2014 · IF 2.016 · 发表于 2014 年 8 月 11 日
作者: Xiao-Yu Ding,Lai-Ma Luo,Ze-Long Lu,Guang-Nan Luo,Xiao-Yong Zhu,Ji-Gui Cheng,Yu-Cheng Wu
阅读全文 在 PubMed 查看

摘要

Pr 2 O 3 doped W composite were synthesized by a novel wet chemical method and spark plasma sintering. The grain size, relative density and the Vicker hardness HV 0.2 of Pr 2 O 3 /W samples were 4   μm, 98.3% and 377.2, respectively. The tensile strength values of Pr 2 O 3 /W were higher than those of pure W. As the temperature rises from 25   °C to 800   °C, the conductivity of pure W and W–1   wt% Pr 2 O 3 composites decreased with the same trend, was above 150   W/m   K.