A series of (Ti 0.5 Nb 0.5 )C-x wt.% SiC (x = 0, 5, 10, 20) composites were prepared by spark plasma sintering . Dense microstructures with well‐dispersed SiC particles were obtained for all composites. With the increment of SiC content, the Vickers hardness , Young's modulus and fracture toughness increase monotonically. An optimized flexural strength of 706 MPa was achieved in (Ti 0.5 Nb 0.5 )C-5 wt.%SiC composite. (Ti 0.5 Nb 0.5 )C-20 wt%SiC composite exhibits the highest fracture toughness of 6.8 MPa m 1/2 . The crack deflections and the suppression of grain growth were the main strengthening and toughening mechanisms. Besides, (Ti 0.5 Nb 0.5 )C-20 wt%SiC composite exhibit the highest thermal conductivity of 45 W/m·K at 800 °C.