Ni3+-Enriched Nickel Sulfide Catalysts for Urea Oxidation

Journal 2026 · IF 11.8 · 发表于 2026 年 5 月 20 日
作者: Qiu Ren,Nathan Delaney,Zhen Liu,Cassidy Tran,Samuel Eisenberg,Angel Maqueda Alvarado,Cheng Zhu,Yanqing Xin,Denghui Zhang,Guizeng Liang,Tianyi Kou,Xiao Wang,Yat Li
阅读全文 在 PubMed 查看

摘要

The urea oxidation reaction (UOR) offers a low-energy alternative to the oxygen evolution reaction (OER) for hydrogen generation while simultaneously enabling urea-rich wastewater remediation. However, most nickel (Ni)-based catalysts rely on in situ oxidation of Ni 2+ to Ni 3+ , the actual active species, requiring high anodic potentials and resulting in substantial overpotentials. Here, we introduce a simple yet effective strategy to intrinsically enrich Ni 3+ content in nickel sulfide (Ni 3 S 2 ) by adjusting sulfur precursor concentration during hydrothermal synthesis. This approach yields a Ni 3 S 2 catalyst with an increased Ni 3+ /Ni 2+ ratio, achieving a UOR current density of 100 mA cm −2 at only 1.361 V vs. RHE. Density functional theory (DFT) calculations reveal that sulfur-modulated Ni 3 S 2 surface provides a more energetically accessible pathway for C─N bond cleavage compared to sulfur-free Ni(OH) 2 , and that increasing the Ni 3+ /Ni 2+ ratio within the sulfide framework further lowers the energy barrier of the rate-determining step. These results highlight the critical role of sulfur in defining the catalytic scaffold and modulating Ni oxidation states. Furthermore, integrating the catalyst with a 3D-printed interpenetrating device architecture and flow-cell system markedly enhances mass transport and overall performance. This work highlights sulfur-enabled Ni valence modulation as an effective route to advance UOR kinetics and demonstrates the synergy between catalyst design and device engineering for sustainable hydrogen generation coupled with wastewater remediation.